Re-based Diffusion Barrier on A Ni-based Superalloy / Najlacnejšie knihy
Re-based Diffusion Barrier on A Ni-based Superalloy

Code: 09198060

Re-based Diffusion Barrier on A Ni-based Superalloy

by Wang Yongming

The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat to power, and improving its efficiency is a ceaseless task. The most practical route to increase the efficiency is to increase th ... more

46.25

RRP: 54.23 €

You save 7.98 €


In stock at our supplier
Shipping in 5 - 8 days
Add to wishlist

You might also like

Give this book as a present today
  1. Order book and choose Gift Order.
  2. We will send you book gift voucher at once. You can give it out to anyone.
  3. Book will be send to donee, nothing more to care about.

Book gift voucher sampleRead more

More about Re-based Diffusion Barrier on A Ni-based Superalloy

You get 112 loyalty points

Book synopsis

The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat to power, and improving its efficiency is a ceaseless task. The most practical route to increase the efficiency is to increase the maximum operating temperature. Over the past several decades, the improvement of this temperature was constantly attained by the developments of thermal barrier coating and superalloys, but almost reached a limit because the microstructural deterioration of both the base superalloy and the coating system due to the interdiffusion between them can be dramatically aggravated by further increasing temperature. The novel diffusion barrier type bond coat, therefore, is a solution to this issue. This book introduces how to form a rhenium-based diffusion barrier on a nickel-based superalloy. The formation process and thermal stability of the diffusion barrier are discussed through analyzing its macro- and micro-structures by XRD, EBSD, EPMA, SEM, and TEM, etc. This work provides the fundamental knowledge about the novel coating system, and should be especially useful to researchers and students in high-temperature materials science and technology.

Book details

Book category Books in English Technology, engineering, agriculture Technology: general issues

46.25

Trending among others



Collection points Bratislava a 13253 dalších

Copyright ©2008-26 najlacnejsie-knihy.sk All rights reservedPrivacyCookies


Account: Log in
Všetky knihy sveta na jednom mieste. Navyše za skvelé ceny.

Shopping cart ( Empty )

For free shipping
shop for 59,99 € and more

You are here: